High temperature
PEEK Wafer Cassette
25-slot carrier for 4″ and 6″ wafers. Holds slot geometry through hot DI water, acid benches and bake steps where PP creeps and warps.
- 4″ / 6″Wafer size
- 25Slots
- 250°CContinuous use
- ESD option104–1011 Ω
25-slot PEEK, PFA and PP carriers engineered to SEMI dimensions — particle-controlled, ESD-safe and cleanroom-ready. Specify your wafer size, process temperature and automation interface; we deliver a qualified carrier, not a compromise.
Choose the resin that matches your process — high-temperature PEEK, ultra-clean PFA, or cost-efficient PP for ambient storage and shipment. All three share the same slot geometry, so a wafer can move between them without re-teaching your tools.
High temperature
25-slot carrier for 4″ and 6″ wafers. Holds slot geometry through hot DI water, acid benches and bake steps where PP creeps and warps.
Transport
Rigid outer box with top and bottom lids that locks the cassette in place. ESD ABS body, particle-free foam-free interior, 24-month service life.
Ultra clean
Translucent white PFA carrier for the most aggressive wet chemistries. Lowest extractables of the three resins, with visual inspection of every slot.
A carrier is not a container. It is a metrology reference, a chemical vessel and a robot interface at the same time. These are the six properties we design and inspect for.
PEEK keeps its modulus and slot pitch to roughly 250 °C. Polypropylene starts to soften near 100 °C, so slots drift after a hot bath and wafers begin to touch. Our PEEK bodies are annealed after machining to release residual stress.
Slot edges are radiused and polished, not sheared. Every part is ultrasonically cleaned in DI water, nitrogen-dried and particle-counted before it is bagged, so the carrier enters your line clean instead of being cleaned by your line.
Conductive and dissipative compounds are bulk-loaded, not coated, so surface resistivity of 104–1011 Ω does not wash off or wear through. Essential for compound semiconductors, laser diodes and thin-film devices.
PEEK and PFA resist most acids, bases and solvents used in wafer cleaning. We will tell you where the limit is: concentrated HF attacks PEEK, so for that bath we quote PFA or PTFE instead of upselling the wrong resin.
Robotic flange, bottom-pick and side-handle features can be added to the same body. Slot pitch and datum faces follow SEMI conventions for 100 mm and 150 mm wafers, so the cassette drops into existing load ports without re-teaching.
Slot position, pitch, flatness and wafer seating are checked on a CMM and recorded per lot. You receive the inspection report with the shipment — a number you can put in your incoming quality file, not a brochure promise.
Polypropylene made the semiconductor carrier affordable. It did not make it dimensionally stable.
PP softens at roughly 100 °C, creeps under load and sheds particles as it wears. In an ambient stocker that is acceptable. In a hot DI rinse, an acid bench, a bake step or a plasma-adjacent environment, the same carrier relaxes, slot pitch changes and wafers that were safely separated start to touch.
PEEK solves that specific failure. Its glass transition is about 143 °C and its continuous service temperature around 250 °C, so a cassette that leaves a 90 °C bath returns to the same dimensions it had before. Lower outgassing and lower wear debris follow from the same molecular structure.
When PP is the right answer: ambient storage, outgoing shipment and single-use logistics, where cost dominates and temperature never exceeds 60 °C. We supply both, and we will say so.
| Property | PP | PEEK | PFA |
|---|---|---|---|
| Continuous service temp. | ~100 °C | ~250 °C | ~260 °C |
| Glass transition (Tg) | −10 °C | 143 °C | −90 °C |
| Density | 0.90 g/cm³ | 1.30 g/cm³ | 2.15 g/cm³ |
| Tensile strength | ~30 MPa | ~100 MPa | ~28 MPa |
| Creep resistance when hot | Poor | Excellent | Good |
| Particle shedding | Moderate | Low | Very low |
| Outgassing | Higher | Low | Lowest |
| Concentrated HF | Resistant | Not recommended | Resistant |
| Optical transparency | Clear | Opaque | Translucent |
| Relative material cost | 1× | 15–25× | 8–12× |
| Best fit | Storage, shipment | Hot / aggressive process | HF, ultra-clean wet |
Typical unfilled resin values for comparison only. Actual figures depend on grade, filler and moulding. Certificates of analysis are supplied with each lot.
From 100 mm pilot lines to 200 mm production fabs, the same design rules apply: protect the front surface, keep the pitch, survive the chemistry.
In-process transport, wet bench handling, stocker storage and shipping of monitor wafers.
GaAs, GaN, InP and SiC lines where ESD control and chemical inertness decide yield.
IGBT, MOSFET and diode fabs handling thin, warped wafers that punish poor slot support.
Small-die, high-mix runs needing frequent cassette changes and tight particle control.
Pilot lines and university cleanrooms that need small quantities and custom slot layouts.
Reticle and photomask storage, plus carriers for sapphire, quartz and glass substrates.
Names are withheld under NDA. Process data is reported exactly as the customer recorded it.
A power-device fab in eastern China was losing wafers to edge scratches after a 90 °C rinse followed by a 25-slot PP cassette transfer. Slot pitch on the PP carriers had drifted by 0.4 mm after three months in service.
We replaced the PP bodies with annealed 6-inch PEEK cassettes, keeping the existing outer boxes and load-port interface so no tooling change was needed. Slot pitch is now verified per lot at ±0.1 mm.
A photonics manufacturer moved 6″ × 6″ × 0.25″ masks between two sites every week. The previous wooden crate required a full inspection on arrival and consumed a cleanroom technician for half a day.
We supplied an ESD ABS reticle box with a positive latch and a moulded cavity that holds the mask off its patterned face. Arrival inspection dropped to a visual check, and the box has been in weekly rotation for 18 months.
Dimensions below are from our controlled drawings. Tolerances, resin grade and surface finish can be tightened on request; tell us which value your process actually depends on.
| Parameter | Value |
|---|---|
| Wafer size | 4 inch (Ø100 mm) |
| Slot count | 25 |
| Slot pitch | 4.76 mm (3/16″), SEMI-compatible |
| Outside dimensions | 142.0 (L) × 125.5 (W) × 114.5 (H) mm |
| Weight | 356 g |
| Body material | PEEK, unfilled natural or ESD compound |
| Colour | Natural tan / black (ESD) |
| Continuous service temperature | up to 250 °C |
| Slot position tolerance | ±0.10 mm |
| Surface resistivity (ESD grade) | 104 – 1011 Ω |
| Handling features | Robot flange, side handles, bottom pick (option) |
| Matching outer box | PP shipping box with top and bottom lids |
| Cleaning | Ultrasonic DI, nitrogen dry, particle count |
| Packing | Double bagged, cleanroom film, export carton |
| Parameter | Value |
|---|---|
| Wafer size | 6 inch (Ø150 mm) |
| Slot count | 25 |
| Slot pitch | 6.35 mm (0.25″), SEMI-compatible |
| Outside dimensions | 142.0 (L) × 177.4 (W) × 171.3 (H) mm |
| Weight | 369 g |
| Body material | PEEK, unfilled natural or ESD compound |
| Colour | Natural tan / black (ESD) |
| Continuous service temperature | up to 250 °C |
| Slot position tolerance | ±0.10 mm |
| Surface resistivity (ESD grade) | 104 – 1011 Ω |
| Handling features | Robot flange, side handles, bottom pick (option) |
| Matching outer box | PP shipping box with top and bottom lids |
| Cleaning | Ultrasonic DI, nitrogen dry, particle count |
| Packing | Double bagged, cleanroom film, export carton |
| Parameter | Value |
|---|---|
| Compatible cassette | 4 inch or 6 inch, 25-slot |
| Configuration | Top and bottom lid, snap latch |
| Body material | PP, virgin or ESD compound |
| Colour | Black / natural |
| Stacking | Interlocking ribs, 5 high loaded |
| Service temperature | −10 to 60 °C (transport) |
| Closure | Tool-free latch, tamper evident option |
| Interior | Foam-free, wafer-safe, no loose liner |
| Marking | Laser-marked part number and lot |
| Packing | Double bagged, export carton |
| Parameter | Value |
|---|---|
| Wafer size | 4 inch (Ø100 mm); 6 inch on request |
| Slot count | 25 |
| Body material | PFA, virgin, unpigmented |
| Colour | Translucent white |
| Continuous service temperature | up to 260 °C |
| Chemical resistance | Acids, bases, solvents incl. concentrated HF |
| Extractables | Ultra-low; suitable for critical wet cleans |
| Inspection | Visual slot check through translucent body |
| Cleaning | Ultrasonic DI, nitrogen dry, particle count |
| Parameter | Value |
|---|---|
| Reticle format | 6 × 6 × 0.25 inch (152.4 mm square) |
| Capacity | Single reticle |
| Body material | ABS (ESD) |
| Weight | 380 g (empty) |
| Service life | 24 months |
| ESD performance | Dissipative; protects mask from CDM events |
| Contact design | Mask supported off the patterned face |
| Closure | Positive latch, tool-free |
| Application | i-line stepper masks, storage and inter-site shipment |
Dimensions are nominal for the catalogue part. Custom envelopes, slot counts and wafer sizes (including 8″ / 200 mm) are available — see custom manufacturing.
You do not need a finished 3D model. Six numbers and a description of your process are enough for us to start.
From that we return a DFM review, a material recommendation, a price and a lead time within 24–48 hours. Machined prototypes start at 10 pieces; moulded production becomes economic from roughly 500 pieces.
Wafer size, slots, envelope, chemistry and interface. A sketch is enough.
We flag thin walls, draft angles and handling conflicts, then price it.
Machined sample with a CMM report for fit check on your tool.
Moulding or machining, 100% dimensional and particle inspection.
| Catalogue sample | 3–7 working days |
| Custom machined sample | 10–15 working days |
| New injection mould | 25–35 days |
| Production run | 15–25 days after approval |
Shanghai Xinkehui New Materials Co., Ltd. develops and manufactures semiconductor materials and handling hardware — sapphire substrates, silicon and silicon carbide wafers, quartz and ZnSe optics, and the polymer carriers that move wafers between process steps.
We started on the materials side, which is why our carriers are specified by resin grade and measured by dimension rather than described by adjective. Our engineering team works directly with fab process engineers: if a cassette fails, we want the bath temperature, the soak time and the particle map, not a purchase order for a replacement.
Manufacturing is based in Shanghai with partner production in Xiamen, and we ship to customers across Asia, Europe and North America. Every order leaves with a dimensional inspection report, a material certificate and a lot number that can be traced back to the resin batch.
Certificates are available as scanned copies for your supplier qualification file — ask us and we will send the current versions.
Capability overview — photographs of our Shanghai and Xiamen facilities are supplied on request and during customer audits.
Send your drawing or your process description and you will get a technical reply — including where a PEEK cassette is the wrong choice.
Contact the technical teamCarrier qualification is slow enough already. These are the commitments we make so that trying us costs you time, not money.
Standard catalogue cassettes and boxes, free of charge for qualified customers. You pay freight only.
Sample freight is credited against your first production order, so evaluation ends up costing nothing.
Any dimensional or material defect within 30 days: replacement or refund, return freight on us.
Technical questions answered within one working day, in English or Chinese, by the engineer handling your file.
Customers audit our line before they qualify a carrier, and we prefer it that way. Walk the machining floor, watch a CMM run, and open a random carton from stock. Visits can be arranged at our Shanghai office and the Xiamen production site — tell us your dates and we will plan the schedule, including pickup from Pudong or Hongqiao.
Fourteen answers on material choice, dimensions, cleaning and logistics. If yours is not here, send it — we answer technical questions whether or not you buy.
Ask a questionA cassette is a slotted carrier that holds wafers upright and separated during transport, storage and wet processing. Each slot keeps a fixed pitch so wafers never touch, protecting the polished front surface and edges from scratches, particles and cross-contamination.
PEEK holds its dimensions and stiffness to about 250 °C, while polypropylene softens near 100 °C. That means no slot creep after hot DI water, acid or bake steps, plus lower particle shedding and outgassing. For ambient storage and shipping, PP is still the cost-effective choice — we supply both.
Yes. Standard tooling covers 25-slot 4-inch (100 mm) and 6-inch (150 mm) cassettes, and we also produce 200 mm and custom-pitch versions. Standard pitch is 4.76 mm for 4-inch and 6.35 mm for 6-inch wafers.
We supply insulating natural PEEK and permanently conductive or dissipative compounds with surface resistivity of 104–1011 Ω. The additive is in the bulk resin, so performance does not wear off. ESD grades are recommended for compound semiconductors and laser diodes.
Yes. Send wafer size, slot count, pitch, envelope, robot or load-port interface, and the chemicals and temperatures involved. We return a DFM review and quotation in 24–48 hours, then produce a first article for approval before mass production.
Catalogue 4-inch and 6-inch PEEK cassettes typically start at 50 pieces. Custom machined designs start from 10 pieces. Evaluation samples of one to five pieces are available.
Catalogue samples ship in 3–7 working days. Custom machined samples take 10–15 working days after drawing approval. A new injection mould takes 25–35 days.
Yes — standard catalogue items are free for qualified customers; you cover courier freight, which we credit against your first production order.
Every part is ultrasonically cleaned in DI water, nitrogen-dried, dimensionally inspected and particle-counted, then double-bagged in cleanroom film inside an export carton. Class 100 cleanroom bagging is available on request.
Unfilled PEEK serves continuously around 250 °C, with a glass transition near 143 °C and melting near 343 °C. PFA is rated to about 260 °C with lower extractables. PP should stay below roughly 100 °C.
PEEK resists most acids, bases and solvents but is attacked by concentrated hydrofluoric acid and some strong oxidisers. For concentrated HF, choose PFA or PTFE. Tell us your chemistry and we will recommend the right resin instead of the most expensive one.
We ship worldwide from Shanghai by express, air and sea. Terms are typically EXW, FOB Shanghai or DDP by negotiation. Export documents, material certificates and inspection reports accompany every shipment.
We replace or refund any part with a dimensional or material defect within 30 days of delivery, and cover return freight when the fault is ours. Custom parts are covered against deviation from the approved drawing.
Yes. The 25-slot PP shipping box with top and bottom lids is sized for 4-inch and 6-inch cassettes, with ESD and cleanroom bagging options, so cassette and outer box arrive as one qualified set.
Tell us your wafer size, process temperature and chemistry. We will tell you which resin survives it, what it costs, and how fast it can ship.
Attach nothing and write three lines — that is enough to start. For drawings, email us directly and we will reply with a DFM review.